Typical Values
Typical values of the limit (Se) for steels are 1/2 the ultimate tensile strength, to a maximum of 100 ksi (690 MPa). For iron, aluminium, and copper alloys, Se is typically 0.4 times the ultimate tensile strength. Maximum typical values for irons are 24 ksi (165 MPa), aluminums 19 ksi (131 MPa), and coppers 14 ksi (96.5 MPa). Note that these values are for smooth "un-notched" test specimens. The endurance limit for notched specimens (and thus for many practical design situations) is significantly lower.
Read more about this topic: Fatigue Limit
Famous quotes containing the words typical and/or values:
“A building is akin to dogma; it is insolent, like dogma. Whether or no it is permanent, it claims permanence, like a dogma. People ask why we have no typical architecture of the modern world, like impressionism in painting. Surely it is obviously because we have not enough dogmas; we cannot bear to see anything in the sky that is solid and enduring, anything in the sky that does not change like the clouds of the sky.”
—Gilbert Keith Chesterton (18741936)
“During our twenties...we act toward the new adulthood the way sociologists tell us new waves of immigrants acted on becoming Americans: we adopt the host cultures values in an exaggerated and rigid fashion until we can rethink them and make them our own. Our idea of what adults are and what were supposed to be is composed of outdated childhood concepts brought forward.”
—Roger Gould (20th century)