Dip Soldering - Process Schematic

Process Schematic

The workpieces to be joined are treated with cleaning flux. Then the workpiece is mounted in the workholding device and immersed in the molten solder for 2 to 12 seconds. The workpiece is often agitated to aid the flow of the solder. The workpiece holder must allow an inclination of 3 to 5 deg. so that the solder may run off to insure a smooth finish.

Read more about this topic:  Dip Soldering

Famous quotes containing the word process:

    Rules and particular inferences alike are justified by being brought into agreement with each other. A rule is amended if it yields an inference we are unwilling to accept; an inference is rejected if it violates a rule we are unwilling to amend. The process of justification is the delicate one of making mutual adjustments between rules and accepted inferences; and in the agreement achieved lies the only justification needed for either.