Material n K (MPa)
Low-carbon steel (annealed) 0.21 600
4340 steel alloy (annealed) 0.12 2650
304 stainless steel (annealed) 0.44 1400
Copper (annealed) 0.44 530
Naval brass (annealed) 0.21 585
2024 aluminum alloy (heat treated—T3) 0.17 780
AZ-31B magnesium alloy (annealed) 0.16 450