Coating of Superalloys
Superalloy products that are subjected to high working temperatures and corrosive atmosphere (such as high pressure turbine region of jet engines) are coated with various kinds of coating. Mainly two kinds of coating process are applied: pack cementation process and gas phase coating. Both are a type of chemical vapor deposition (CVD). In most cases, after the coating process near-surface regions of parts are enriched with aluminium, the matrix of the coating being nickel aluminide.
Read more about this topic: Superalloy
Famous quotes containing the word coating:
“The world is eaten up by boredom.... You cant see it all at once. It is like dust. You go about and never notice, you breathe it in, you eat and drink it. It is sifted so fine, it doesnt even grit on your teeth. But stand still for an instant and there it is, coating your face and hands. To shake off this drizzle of ashes you must be for ever on the go. And so people are always on the go.”